Method for mfg. Al-Sr intermediate alloy


Application Number: 00110851
Application Date: 2000.01.24
Publication Number: 1307144
Publication Date: 2001.08.08
Priority Information:
International: C22C21/00;C25C3/36
Applicant(s) Name: Shandong Polytechnical Univ.
Address:
Inventor(s) Name: Bian Xiufang;Zhang Zhonghua;Chen Junhua
Patent Agency Code: 37205
Patent Agent: zhang xihua
Abstract The present invention relates to metal material. Al-Sr intermediate alloy is manufactured through the steps of: mixing industrial pure strontium carbonate, aluminium oxide, potassium borofluoride and potassium chloride in a certain proportion, putting the material on the surface of molten aluminium, powering the molten aluminium with DC current for 20-60 min and final casting molten aluminium in metal mold or casting and rolling into string. The intermediate alloy has excellent Al-Si alloy modifying effect.