Stress corrosion resistant low-alloy pipe cluster of air cooler


Application Number: 00106074
Application Date: 2000.04.20
Publication Number: 1271840
Publication Date: 2000.11.01
Priority Information:
International: F28D1/00;F28D1/04;F28D1/06;F28F1/18
Applicant(s) Name: Shu Runtao
Address:
Inventor(s) Name: Shu Runtao
Patent Agency Code: 00000
Patent Agent:
Abstract The present invention relates to an air cooling system used in petro-chemical and electric power fields. The low-alloy (12Cr2AlMoV) sheet material and finned tubes, which can resist the stress corrosion of H2S and HCl to improve the anticorrosion performance of air cooling type heat exchanger and elongate service life of equipment. Its advantages are low cost of equipment and low expense in maintenance.