Tag Archives: wear-resistant

Low-carbon martensite heat-treating process for hot-rolled high-strength wear-resistant steel rail or I-steel

Application Number: 00117811Application Date: 2000.05.22Publication Number: 1274760Publication Date: 2000.11.29Priority Information: International: C21D9/04Applicant(s) Name: Tang TieqinAddress: Inventor(s) Name: Tang Tiein;Tang XingangPatent Agency Code: 00000Patent Agent: Abstract Steel rail or I-steel of low-carbon alloy steel is treated to acquire self-tempering feature and high strength and wear resistance. The steps include quenching at 800-1100 deg.c by utilizing the… Read More »

Reinforced floor with ultrahigh wear-resistant and steeping-resistant property and making method thereof

Application Number: 00123774Application Date: 2000.09.07Publication Number: 1285449Publication Date: 2001.02.28Priority Information: 2000/8/3 CN 00120864.0International: B32B5/14;E04F15/02Applicant(s) Name: Feng XiaohuanAddress: Inventor(s) Name: Feng Xiaohuan;Cui GuifangPatent Agency Code: 13101Patent Agent: meng shuxunAbstract The superhigh wear-resisting and water-proofing strength floor is characterized by that its wear-resisting layer is a glued paper layer made up by impregnating pure wood pulp paper… Read More »